Technical Index
|
Natural Rubber (-40ºC-60 ºC)
|
Neoprene Rubber(-25ºC-60ºC)
|
||
Hardness(IRHD)
|
60±5
|
60±5
|
||
Tensile Strength(MPa)
|
≥18
|
≥17
|
||
Elongation at Break(%)
|
≥450
|
≥400
|
||
Brittleness Temperature(ºC)
|
≤ -50
|
≤ -40
|
||
Compression Set(70ºC×24h)(%)
|
≤ 30
|
≤ 15
|
||
Ozone Aging Resistance(20% strain,40ºC × 96h)
|
25 pphm
|
100 pphm
|
||
No Cracks
|
No Cracks
|
|||
Hot Air Aging
|
Test Condition(ºC × h)
|
70 × 168
|
100 × 70
|
|
Max Change in Tensile Strength(%)
|
- 15
|
-15
|
||
Max Change in Elongation at Break(%)
|
- 20
|
-40
|
||
Max Change in Hardness(IRHD)
|
-5 , +10
|
0 , +10
|
||
Bond Strength Between Elastomer and Steel Plate(KN/m)
|
>10
|
>10
|
||
Bond Strength Between Elastomer and PTFE(KN/m)
|
>7
|
>7
|